Blog / Bitumen 60/70 vs 80/100
Short answer: Use 60/70 for hot climates and heavy traffic, and 80/100 for cooler climates where a softer binder resists cracking.
| Property | 60/70 | 80/100 |
|---|---|---|
| Penetration @ 25°C | 60–70 dmm | 80–100 dmm |
| Softening point | 48–56 °C | 42–51 °C |
| Hardness | Harder | Softer |
| Best climate | Warm and hot | Cool |
| Resists | Rutting | Cracking |
The two numbers show how far a standard needle sinks into the bitumen in tenths of a millimetre. Check which grade your road design calls for.
See full specifications and datasheets: Bitumen 60/70 and Bitumen 80/100.
Tell us the grade, quantity in tonnes and delivery location. We reply within 24 hours.